I wondered if anyone who does tig or mig welding of very thin stainless have used a product called Solar Flux to stop sugaring instead of purging or heat sinks.
It is an American product developed years ago for weld repairs of jet engines.
Have read good and bad reports on the net.
It leaves a ceramic coat on the back of the weld and can be hard to get rid of.
Is there any similar products on the UK market that are not as pricey 1lb £75.
As a newby to tig (Brief time 25years ago on car bodywork) its an enjoyable learning curve.
Jody on an American Website has been very helpful
link in how to do the many types of electric welding.
Windy